Document oM73EZEpvpjkrr6XmDvbpKJ2X
PLAINTIFF'S EXHIBIT
I UC-3649
Tomoe Engineering Company. Ltd
KAIK OKFICCi OAfKt MARjlEW aUfVDtNS **. NIHOM*AHI 3<HOMI, CNUO'KU
TOKYO, JAPAH
(ANNEX OFFICE) SHIN SHIN KAIKAN BUILDING 14-1, NIHONBASHI 3-CHOME, CHUO-KU
TOKYO, JAPAN
CAOLt ADONIII "lOMOT" tilixi otjjoaoa cowot tok TKVtRHONI j TOKYO
Date of Call: February 26, 1973
Customer:
DIC, Sakai Plant
Interviewed Person:
Mr. N. Narisada, The 4th Technical Group
Visited by:
Messrs.
J. L. Myers - UCC F. S. Wada - UCSEL H. Fukuma - TEC T. Mito - TEC
RG-244 Toxicology:
Explained and provided information centralized on, "The Safe Use of Calidria RG-244". Subject company expressed desire that they wanted to take actual airborne measurements.
Received following questions on RG-244.
1. What is best method for adding RG-244 based upon master batch method?
Answer:
In the States all deliveries are made in 10 pound bags and they are thrown-in as is. There is no company adding RG-244 under the master batch method.
2. Method of Distribution.
Answer: Explained distribution by methods of Cowels, Sonolator and Vortex mixer.
3. On boiling water resistance.
Answer:
As they are not as critical in the States as in Japan, we have not received such
complaints. Recommend RG-244-A-174 or 187
treatment. Delivered and requested test to be conducted RG-244 silane treated by Tomoe.
UCC 008556
4. Bubbling Problem.
Answer:
In case RG-244 is added to polyester resin. as compared to Aerosil since it is more transparent the bubbles can be seen more readily. In actuality as compared to Aerosil it does not mean that more bubbles exist. As the specific gravity is close to double that of Aerosil, in fact we believe less bubbles exist.
5. Spray Gun Plugging Problem.
Answer: Explained case history of;
Ronningen Petter GAF Basket type Cuno Auto-Clean Cuno Mikro-Wynd II
60 mesh
60 mesh
50 mesh 350M {- 45 mesh)
6. Reference RG-244, glass fiber and polyester resin, if available desire to have data on impregnation.
Answer:
As compared to Aerosil, RG-244 is better in impregnation, however, no data available..
7. Is RG-244 being used for gel coat in the States?
Answer:
Some is being used, however, as use potential is small it is not being aggressively promoted in the States. The manufacturing process of the subject plant differs a bit from that of the Chiba Plant, but from a technical standpoint practically all problems have been solved.
It was stated that upon confirming the actual amount to be used at Chiba Plant decision will be made whether usable or not.
2 UCC 008557