Document garqD8m7nX3pQKGGpqK7jRX4e

R-120 R Preliminary tests Indicated the coating to be zinc oxide. Earlier laboratory bench and dynamometer tests have abeam zinc to produce torque fluctuations above 510*F vhen zinc smears onto the cast iron, then oxidizes to provide a relatively durable and high friction local coating. The Bendlx lining appears to have about half the zinc content of the Delco lining and also contains enough abrasive to remove any zinc oxide coatings. Thus it vould be expected that the Delco lining should he more prone tevard producing brake roughness. The problems srudden appearance after much prior vehicle testing probably vas due to the accelerated fora of the latest vehicle testing, the brakes being used repeatedly producing high temperatures before the linings seated fully. Our tests shoved this exaggerates the roughness. Also the nev corporate L-l disc brake caliper assembly is much more rigid so more stops are required to achieve full seating and uniform lining pressure. Car Engineering vas informed of our findings and has specified that the Bendlx material be used until more vehicle evaluations are completed vlth seated linings. Further reductions of brake roughness vere required on the- 1972 Thunderbird. Dynamometer tests of early production JGelsey-Hayes rotors shoved permanent runout changes after a fev brake applications. This vas found to have been caused by high surface residual stresses (about 10,000 psl) from the final grinding operation. However, the runout itself did not cause the torque variations. The brake roughness resulting from the rotor appears to result from both the rotor thickness variation ami its surface finish. It vas found that a lathe turned rotor provides lover brake roughness and lover initial brake effectiveness, hovever, the latter corrects Itself vlth use. Production rotors now are using a lathe turned finishing operation vlth lov thickness variation limits (.0002" maximum rather than the previous .0005")- PRODUCED BY FORD IN V P?D - OGf i