Document ZByzYL1MZ6kVdzmqNzBG3ZpkO
Monsanto
FROM (NAME & LOCATION >
J. H. Orem - Galt Labs - 1730
March 2, 1977 TANCO ADHESIVES
C/R 2-7-77
TO
J. A. Cannon T. G. Iversen - B3NC D. R. Kenner - Marietta, Ga, L. 0. Raether - B3NB N. W. Touchette J. S. Williams - 1940
Two possibilities for replacing KP-140 are Santicizer B-16 and
Santicizer 141. Of the two, I think B-16 would bite into the
polypropylene better and, thus, provide a stronger adhesive bond.
Also, I feel more comfortable with a phthalyl glycolate than I do
with a phosphate for FDA type applications.
,
Why do they use Benzoflex 50 (200-300M pounds) for bookbinding adhesives rather than Santicizer 160? Is it to maintain dual sources of supply for plasticizers, or is there a technical/eco nomic reason?
JHO/gls
cc "o
T<STX
STLCOPCB4092558