Document QJpwO3O95LRzD0npepo272m0R

PLAINTIFF'S EXHIBIT UC-990 MEMORANDUM cc\ Subject: Relationship of RG-244 to FMC German Patent 1,567,517 and U. S. Patent 3,458,393. RG--244 It is understood that the following is the current pro cedure for producing RG-244: 1. High purity asbestos is heated at about 100F. and subjected to grinding and cyclone separation. 2. The separated asbestos material is introduced into a tank (with no additional heating) and sodium silicate at ambient temperature is also added. The pH at this point goes to about 10.5. 3. Acetic acid is next added (without heating) to reduce the pH to about 7.5 to 8, whereby silica is precipitated onto the asbestos material to provide a material having a siliceous outer layer. 4. The wet material is pressed, dried and then dry ground to provide a material having about the same fineness as the starting asbestos material. FMC German Patent 1,567,517 The claims (copy attached) of German patent 1,567,517 describe a process wherein chrysotile asbestos is heated with an acid whereby the Si02/Mg0 ratio of the asbestos is changed from 1:1 to from 1.05:1 to 1.3:1. Conclusion re FMC German Patent 1.567,517 In view of the fact that the production of RG-244 does not involve heating asbestos with an acid, German Patent 1,567,517 is not infringed. FMC U. S, Patent 3,458,393 This patent claims an article of manufacture and a process for making the article of manufacture. The article of manu facture claim recites a "chemically modified chrysotile at least 5% by weight having a particle size not exceeding one micron and being characterized in having a Si02/Mg0 weight ratio of from about 5% to about 30% greater than the corresponding ratio of the parent chrysotile." The process claim of U. S. P. 3,458,393 recites a "method of treating chrysotile which comprises subjecting it to the action of an acidic solution for a time and at a temperature sufficient to increase the Si02 to MgO weight ratio from about 5% to about 30% and mechanically attriting the treated chrysotile until at least 5% by weight has been reduced to a particle size not exceeding about one micron." Conclusion re FMC U. S. Patent 3,458,393 There is no infringement of the process claim of U.S.P. 3,458,393 since chrysotile is not subjected to an acidic solution 2. during the making of RG-244. The lowest pH achieved during processing is 7.5. If the expression "chemically modified" is given its broadest meaning then RG-244 literally infringes the article claim of U.S.P. 3,458,393. However, RG-244 is asbestos having a preci pitation deposited siliceous outer layer. On the other hand U.S.P. 3,458,393 specifically describes and claims a chemically modified asbestos wherein the modification involved is an acid-asbestos reac tion whereby MgO is removed from asbestos. In other words, RG-244 is asbestos to which silica has been added whereas the material of U.S.P. 3,458,393 is asbestos from which MgO has been removed. Con sequently, there is no identity of product between RG-244 and the material of U.S.P. 3,458,393 and hence no infringement. DOS 1, 567,517 Claims: 1. Method for producing a microcrystalline, colloidalmaterial from chrysotile having an SiOg/MgO ratio of 1:1, characterized in that the chrysotile is heated with an acid for such a time and at such a temperature that the S102/MgC ratio is changed, to from 1.05:1 to 1.30:1, whereupon the acid-treated and chemically modified chyrsotile is mechanically comminuted until at least 10 per cent by weight of tne particles have a particle size of less' than 1 my. 2. Method according to Claim 1, characterized in that the resulting microcrystalline, colloidal material is converted tc a stable gel by the addition of a hydrophilic liquid. 3. Method according to Claim 2, characterized in that the stable gel is formed into a film and dried.