Document OB8wyer0QM8L8wZjYNdY7RbK
Disperser/Mixer Improves
Plastisol Production
I he Emigsville, Pa., plant of Herculite Protective Fabrics Corp. has improved production of plastisol adhesives with installa tion of a disperser/mixer from Day Mixing, Cincinnati, Ohio. The Daymax unit turns out a better dispersion and more uniform product in less than half the time of the previous system.
Herculite produces custom vinyl laminates for applications ranging from tarps to hospital mattress ticking. Prior to install ing the Daymax disperser, Hercu lite was using a conventional shear-type mixer, which required about an hour to produce a onedrum (55-gallon) batch of plas tisol. And the company's lamin ating line was being delayed by the plastisol-producing part of the operation. . With the Daymax disperser, a -five-drum batch is prepared in two hours, providing a constant -^supply of plastisol to the lamipisnator and allowing the operator
I
to help out in other areas of the plant. According to Bill Stegner, plant quality control supervisor, "We needed a bigger disperser and we got a good one. It turns out 255 gallons in two hours. The speed and larger quantities we can produce on the disperser re ally helped us, and we get a better dispersion and more uni form product."
Production Process Herculite installed the 330-
gallon (maximum capacity) Daymax about a year ago. The in stallation included a pumping system for adding liquid ingre dients to the mix, an access stand for operator loading of other ingredients through the top opening, and a dust control hood over the top opening where pow dered resin is added to the mix.
The disperser unit, which handles 2,500- to.3,000-cP..plastisol adhesives, is equipped `with . a jacket for. chilled water.^ercu-
lite uses 40 cold water circu
lating in the jacket to offset the
heat generated in the mix.
Precise temperature control is
important, according to Stegner;
without the coolant, the tempera
ture of the mix could rise about
30F within five to seven
minutes, spoiling a batch worth
$2,000. The plastisol is heat-sen
sitive and excess heat cures it.
Another potential problem is that
overmixing causes the plastisol
to jell, and great care is taken to
avoid this.
.
Presently, Herculite has 17 dif
ferent formulations in the same
viscosity range. Since installing
the disperser, the company has
been improving these formula
tions by varying the loading
sequence for plasticizer, resin,
fillers, wetting agents, and other
ingredients. The sequence and
rate of addition is very critical for
better dispersion and control of
heat, rin ,some ^formulations, ^all
-the' plasticizersjs^)ut:igjRfirst,
'ajADHFStVES
DSW 587233
STLCOPCB4092569
r
Table II -- Typical Solution Properties
Approximate viscosity,*cP pH Product solids, % Acrysol ASE-60 Acrysol ASE-75 Acrysol ASE-95
7.0 0.5 2.0
8.0 0.5 2.0
9.0 0.5 2.0
200 65 400
3270 270 2800
215 70 280
3600 200 4500
220 60
90
3500 140 5400
`Measured at 25C on a Brookfield LVF viscometer at 60 rpm; various spindles. These viscosities are |given simply to illustrate relative molecular sizes.
In each case, neutralization was done with concentrated ammonium hydroxide.
Table III --Thickening Efficiency of Acrysol ASE-60 vs. Acrysol ASE-75 for
Typical Aqueous Dispersions
-
System
Nitrile latex2
Styrene copolymer3
Natural latex4
Acrylic latex (Rhoplex B-60A)
Paper coating (Rhoplex B-15)
Rutile Ti02 dispersed with 0.25% Tamol 731
Total solids, %
20 20 50 20 35 10 60
Thickener1
Acrysol ASE-60 Acrysol ASE-75 Acrysol ASE-60 Acrysol ASE-75 Acrysol ASE-60 Acrysol ASE-75 Acrysol ASE-60 Acrysol ASE-75 Acrysol ASE-75
Acrysol ASE-60 Acrysol ASE-75 Acrysol ASE-60 Acrysol ASE-75
% thickener on total solids -- giving Brookfield viscosity (12 rpm) of:
2,000 cP
6,000 cP
10,000 cP
4.0 6.2 4.2 9.0 0.8 0.6 2.5 > 6.0
3.2
5.4 8.0 6.4
>10.0 1.3 2.2 4.1
> 6.0 5.0
6.7 8.0 7.5 > >10.0 1.6 3.5 5.8 > 6.0 --
8.3 >30.0
0.3 0.5
12.0 >30.0
0.5 1.2
15.0 >30.0
0.6 1.7
Solution of sodium salt of polymer indicated. 2Nitrex 2614 -- supplied by Naugatuck Chemical Div. of U.S. Rubber Co. 3Kralac 2733 -- supplied by Naugatuck Chemical Div. of U.S. Rubber Co. 4NC-400 -- a centrifuged natural rubber latex supplied by U.S. Rubber Co.
Acrysol ASE-75 are .also of interest as temporary binders in ceramics and as dispersants and suspending agents for pigments or abrasives.
Films formed from Acrysol ASE-75 or a solution of the polymer salt are hard and somewhat brittle. Unless the carboxyl groups of the polymer are crosslinked during film formation with a zinc-ammonia complex, these films are water-sensitive and may be redis solved in dilute alkali solutions or some organic solvents.
Acrysol ASE-95 Acrysol ASE-95 is also an acid-con
taining, acrylic emulsion copolymer. When diluted with water and neutra lized with a base, each particle dis-
solves. The emulsion clarifies under these conditions and becomes a highly effective thickener. In comparison to Acrysol ASE-60 and Acrysol ASE-75, Acrysol ASE-95 imparts a very leggy consistency to adhesive compounds.
Solutions of this emulsion are par ticularly useful for thickening pigment suspensions, surfactant solutions, polar solvents, and compounded latex adhe sive systems.
Conclusion These acrylic emulsion copolymers
can be incorporated directly into com positions to be thickened without any necessity for slow preliminary prepara tion of separate thickener solutions. Thisin-situ thickening is a marked ad
- ADHESIVES AGE, FEBRUARY 1977
vantage over procedures usually em
ployed with natural thickeners (e.g.,
alginates) or with semisynthetic poly
mers (e.g., methyl cellulose or car-
boxymethyl cellulose). It is usually de
sirable to predilute an Acrysol ASE
emulsion with equal parts of water and
to keep the pH at as low a`value as
possible until the emulsion has been
thoroughly stirred in. Adjustment of
pH to dissolve or swell the thickener
then brings the formulation to the
desired viscosity smoothly and rapidly.
The thickeners offer the following
primary advantages: viscosity control,
ease of mixing, in-situ thickening, and
high solids content. They may be used
in the formulation of a wide variety of
adhesives,
-.. ...
,
DSW 587234
STLCOPCB4092570
Lifting PVC resins in 40- and 50-1 b bags to top of platform in preparation for mixing. Disperser is at right.
followed by resin and then filler; in others, a portion of the plas ticizer will be held off until after all the antimony oxide has been added.
It takes approximately seven minutes for the addition of all ingredients, and the final mix is prepared after about three more minutes.
Quality control is stringent; before any batch is emptied from the equipment, the dispersion is checked carefully for lumps'and viscosity.
The plastisol from the dis perser is cured between vinyl sheets in a laminator for 15 to 18 seconds. The vinyl laminate is then trimmed, tested, inspected, and packaged for shipment.
The Daymax disperser is used four hours a day, five days a week to make 500 mixes or batches per month. No special cleaning is necessary and, according to Stegner, no maintenance has been required to date.
ADHESIVES AGE, FEBRUARY 1977
Here, operator adds wetting agent to the mixer. Dry solids are added at the top
through the funnel-shaped opening. A dust shield has been provided by Herculite on
this machine to create a cleaner environment..
;
v. .
DSW 587235
27
STLCOPCB4092571
The disperser, with a 330-gal maximum capacity and a 300-gal working capacity, is being charged with liquid plasticizer from 55-gal drum.
Disperser Features
: The Daymax disperser consists of a vertical tub-shaped tank with a built-in water jacket for product heating or cooling, a cover with a central loading funnel, a gate valve for product emptying, a support base, and a six-blade ro tating knife-edged impeller that operates at 1,800 rpm. The ac tion of the blades and the tank bottom configuration create im pacts of varying pressure as well as friction actions, which account for the low mix time required for dispersion.
Rotation of the impeller pro duces pressure in the liquid next to the cutting edge of the blade, followed by friction action and a low pressure at the trailing edge of the blade, which is com pressed by the leading edge of the next blade. This succession of compressions and depressions at an impeller tip speed of 9,000 fpm allows dispersion -- with ho mogeneity and particle sizes as small as one or two microns -- in as little as two or three minutes.
The disperser can be operated under a vacuum to remove air from the mix. At Herculite, Stegner says it has not been nec essary to use the vacuum cover because 1) with the drive shaft passing through the bottom of the tank to support the dispersion impeller from beneath the sur face of the mix, there is no possi bility of air being introduced into the mix and 2) a system of large, adjustable, and removable baffles (from one to three as required by the application) prevents horizon tal rotation of the liquid and prevents formation of a vortex and the introduction of air.
According to Day, the unit requires essentially no`mainte nance, except for monitoring the mechanical seal for the impeller drive shaft. "The seal in our Daymax has been in for almost a year," said Stegner, "and we have not had to- replace it yet." And cleaning the unit -- for example, before long shutdowns -- con sists of adding solvent, running the .machine, and rinsing.
; ADHESIVES AGE, FEBRUARY 1977
DSW 587236
STLCOPCB4092572