Document J3NLgpw0m068LaZOpYmzrkB0B
Monsanto
CummingPROM (NAME & LOCATION) Paton - General Offices
date :
March 5> 1970
<==:
SUBJECT
:
S0NNEB0RN/P0LYSULFIDES
REFERENCE
:
TO : .
N. W. Touchette JFQ Research
J. R. Darby - JFQ Research M. W. Farrar - JFQ Research W. F. Waychoff
I met Herb Rosenblatt, group leader for Sonneborn, recently.
1. Aroclor 1248/1234
They use in polysulfides. They claim that the high weight loss they used to get at 100 C with 1248/1254 was due to the use of calcium and other metallic peroxides. No problem at 70-85 C which is now the accepted weight loss temperature. Is this true. Perhaps this is how we can "degrade" these PCBs.
Santicizer'1^0
He claimedr^Ehat Santiclzer 140 and lead peroxide in a C-5 catalyst formulation "smokes" spontaneously, I have been preaching the virtues of Santiclzer l48_/> recently. Will I be responsible for blowing up our friendly formulators?
/dbw
Cumming Paton
DSW 588476 STLCOPCB4093812