Document G5Ey4x3vNk0ZvzYXnZpLZnb64
St. Louis - General Offices
February 16, 1961
Aroclor 1248 Heater
Robert C. Canfield Krummrlch Plant
Dear Bob:
This Is to confirm our conversation of this morning in which you requested information concerning the operation of the 1,000,000 BTU/hr. Aroclor heater in the north area at a bulk temperature of 6l0-620F. I understand that these temperatures are needed only for a two months production run of a special chemical.
I am attaching a copy of a graph showing the change of viscosity vs. time at various bulk temperatures above 600F. obtained by Organic Research using a static steel bomb.
The second graph is a plot showing the maximum fluid life vs. temperature. If the correlation is extrapolated linearly, it indicates that Aroclor is stable up to temperatures -of 620F. The curve also hag been extrapolated to show a stability of approximately 608UF. The actual stability probably lies between the two - extrapolations, however, sufficient data is not available at this time to substantiate any definite point. We do know, however, that the material is infinitely stable at 600F.
The only heater that I know of that is operating above 600F. is a unit at the Hatco Chemical Company, Fords, New Jersey, where the bulk operating temperature is 6lOF. The viscosity of the fluid has increased from 70 SUS to 145 SUS in eight months time. Based on the decomposition data shown on the two graphs, I believe the increase in viscosity is due to the high film temperatures in this heater rather than from the decomposition at the bulk operating temperature. I have been attempting to get the fabricator of the heater to conduct test runs on their heater for quite some time, as I am of the opinion that the heater is not satisfactorily designed for Aroclor.
You might also check with Dave Nelson in the P2S5 area as I understand that he also operates his Aroclor system at tempera tures above 600F. for short periods of time.
01J7SOO
TOWOLDMONOQ54170
Robert C. Canfield
2
February 16, 1961
Since the flux rates in the heater will be very low during the time of operation, X see no apparent reason for not using the heater for this purpose. However, since there is a possibility of a more substantial amount of Aroclor decomposition and HC1 liberation, I would suggest that you continuously vent the system through the vent tank: by taking a full flow through the 1" purge line from the high pressure side of the recirculation line. By all means be sure to keep the moisture below the 100 ppm maximum during operation.
Please let me know if I can be of any assistance to you.
WJDsnlk Attachments
W. J. Davis
0137501
TOWOLDMONOQ54171